This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2014, 5, 1712–1724, doi:10.3762/bjnano.5.181
Figure 1: Output voltage and ASR at low current density, showing sulfur tolerance. Yellow shading denotes 24 ...
Figure 2: Output voltage and ASR, showing typical effects of partially reversible sulfur poisoning. Yellow ba...
Figure 3: Output voltage and ASR, showing sulfur tolerance at a current density below 200 mA·cm−2 (24–192 h) ...
Figure 4: Output voltage and ASR, showing initial sulfur tolerance at high current density, and early cell fa...
Figure 5: Top views of ceria deposition on NiO/GDC anodes. a) Treatment 1 (no coating). b) Treatment 2 (direc...
Figure 6: FIB cross-sections halfway through ceria-coated NiO/YSZ anodes, with superimposed EDXS maps (Ni: gr...
Figure 7: Cross-sectional view of an untreated Ni/GDC anode (treatment 1) after operation. a) SEM image; b) E...
Figure 8: Cross-sectional view of a direct-treated anode (treatment 2) after cell operation. a) SEM image; b)...
Figure 9: Cross-sectional views of the thiol-treated anode (treatment 3) of the cell shown in Figure 2 after operatio...
Figure 10: Cross-sectional view of a sulfonate-treated anode (treatment 4) after operation. a) SEM image; b) E...
Figure 11: Average lifetime energy output of SOFCs (with and without GDC interlayers) tested in sulfur-contain...
Figure 12: Average power over cell lifetime, grouped by anode treatment and anode type, ranked by cumulative H2...